马辉太. 王水水浴消解泡塑吸附电感耦合等离子体质谱测定化探样品中金的条件优化[J]. 分析测试技术与仪器, 2018, 24(2): 97-103. DOI: 10.16495/j.1006-3757.2018.02.006
引用本文: 马辉太. 王水水浴消解泡塑吸附电感耦合等离子体质谱测定化探样品中金的条件优化[J]. 分析测试技术与仪器, 2018, 24(2): 97-103. DOI: 10.16495/j.1006-3757.2018.02.006
MA Hui-tai. Optimization of Determination of Gold in Geochemical Exploration Samples by Inductively Coupled Plasma Mass Spectrometry After Dissolved in Aqua Regia and Adsorbed by Foam Plastic[J]. Analysis and Testing Technology and Instruments, 2018, 24(2): 97-103. DOI: 10.16495/j.1006-3757.2018.02.006
Citation: MA Hui-tai. Optimization of Determination of Gold in Geochemical Exploration Samples by Inductively Coupled Plasma Mass Spectrometry After Dissolved in Aqua Regia and Adsorbed by Foam Plastic[J]. Analysis and Testing Technology and Instruments, 2018, 24(2): 97-103. DOI: 10.16495/j.1006-3757.2018.02.006

王水水浴消解泡塑吸附电感耦合等离子体质谱测定化探样品中金的条件优化

Optimization of Determination of Gold in Geochemical Exploration Samples by Inductively Coupled Plasma Mass Spectrometry After Dissolved in Aqua Regia and Adsorbed by Foam Plastic

  • 摘要: 为了简单、快速地测定化探样品中的金(Au),主要研究了王水水浴消解泡塑吸附,电感耦合等离子体质谱(ICP-MS)测定化探样品中金的方法.经过对前处理过程以及仪器测定过程中影响参数的优化,方法的各项指标均满足分析要求.试验结果:方法的检出限为0.014 ng/g,回收率为91%~102%,通过国家一级标准样品的验证,结果与推荐值吻合,方法的相对标准偏差RSD为3.3%~9.4%.方法适用于化探样品中金的检测.

     

    Abstract: In order to carry out a simple and rapid determination of gold (Au) in geochemical samples, inductively coupled plasma mass spectrometry(ICP-MS) was used after the samples were dissolved in aqua regia and adsorbed by foam plastic. The optimization of the prectreatment process and determination process of the instrument were also discussed. The detection limit was 0.014 ng/g, and the spiked recoveries were in the range of 91%~102%, through the verification using the national standard sample the method meets the requirements of the analysis. The results coincide with the recommended values. The RSD were between 3.3% and 9.4%. The method is suitable for the detection of gold in geochemical exploration samples.

     

/